Introduction to Fundamentals of Corrosion in Gases
By
Marek Danielewski
Marek Danielewski
AGH University of Science and Technology
, Cracow
, Poland
Revising author
Search for other works by this author on:
-
Published:2003
Page range:
87 - 89
Abstract
This article provides an introduction to the fundamentals of corrosion in gases. It tabulates the structures and properties of oxides as well as the physical properties of pure metals.
You do not currently have access to this chapter.
Citation
Marek Danielewski, Introduction to Fundamentals of Corrosion in Gases, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 87–89, https://doi.org/10.31399/asm.hb.v13a.a0003716
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Effects of Metallurgical Variables on Aqueous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Thermodynamics of Gaseous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Failure of Copper Rivets Due to “Gassing”
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Atlas of Microstructures
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Electrochemical Refining
Corrosion: Fundamentals, Testing, and Protection
Solidification Structures of Pure Metals
Metallography and Microstructures
Etchants for Revealing Microstructure
Metallography Principles and Practice
Melting of Glasses and Oxides
Induction Heating and Heat Treatment
Electrical Contact Materials
Metals Handbook Desk Edition (2nd Edition)
Properties of Pure Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials