Abstract
This article provides a discussion on a working principle, the operations, characteristics, capabilities, and applications of electrochemical grinding (ECG). The basic elements of the ECG machine tool are also presented.
You do not currently have access to this chapter.
Citation
V.K. Jain, Electrochemical Hybrid Processes, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 157–159, https://doi.org/10.31399/asm.hb.v13a.a0003598
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Electrochemical Grinding
Machining
Hydrogen Embrittlement Delayed Failure of a 4340 Steel Draw-In Bolt
Handbook of Case Histories in Failure Analysis
Numerical Control
Machining
Electrochemical Allied Processes
Corrosion: Fundamentals, Testing, and Protection
Heat Treating of High-Speed Tool Steels
Heat Treating of Irons and Steels
General Introduction to Machining
Metals Handbook Desk Edition (2nd Edition)