Corrosion Monitoring for Industrial Processes Available to Purchase
-
Published:2003
Abstract
This article describes the criteria for selecting a corrosion-monitoring method used in industrial plants. It provides a detailed discussion on the design, advantages, and disadvantages of plant corrosion-testing program. The basic types of racks used to support and insulate the coupons are also discussed. The analysis of electrical-resistance probes, sentry holes, side-stream loop, electrochemical noise, hydrogen-probe, and process streams are used to monitor and estimate corrosion rates. The corrosion rates can also be estimated by ultrasonic thickness measurements, polarization-resistance measurements, corrosion potential measurements, and alternating current impedance measurements. Corrosion monitoring strategies, such as locations, data analysis, redundancy, and other issues, are discussed. The article concludes with information on the interpretation and reporting of corrosion testing.
Sheldon W. Dean, Corrosion Monitoring for Industrial Processes, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 533–541, https://doi.org/10.31399/asm.hb.v13a.a0003659
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.