Corrosion: Fundamentals, Testing, and Protection
Electrochemical Machining
-
Published:2003
Abstract
This article discusses four subsystems of the electrochemical machining (ECM) system: power source, electrolyte cleaning and supply system, tool and tool-feed system, and workpiece and workpiece-holding system. It describes the theory of ECM and provides information on the electrolytes used in ECM. The article reviews the methods associated with workpiece shape prediction. The procedures and integrated approach for the tool design in ECM are discussed. The article also explains the process control, capabilities, and the limitations of ECM. It concludes with information on the applications of ECM.
Sign in
ASM members
Member Sign InV.K. Jain, Electrochemical Machining, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 143–152, https://doi.org/10.31399/asm.hb.v13a.a0003596
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!