Skip Nav Destination
ASM Handbook
Corrosion: Fundamentals, Testing, and ProtectionAvailable to Purchase
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter
Rubber Coatings and Linings Available to Purchase
-
Published:2003
Page range:
845 - 850
Abstract
This article presents a detailed discussion on the relative performance properties of principal rubber types used in lining applications together with their application, vulcanization and inspection techniques, and material and installation costs.
You do not currently have access to this chapter.
Citation
E. Bud Senkowski, Kenneth B. Tator, Rubber Coatings and Linings, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 845–850, https://doi.org/10.31399/asm.hb.v13a.a0003695
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Stud Arc Welding
Welding Fundamentals and Processes
Failure of a Large Oil Storage Tank
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Guide to Nondestructive Evaluation Techniques
Nondestructive Evaluation of Materials
High-Frequency Welding
Welding Fundamentals and Processes
Standards and Inspection
Practical Induction Heat Treating (Second Edition)
High-Frequency Welding
Welding, Brazing, and Soldering
Forging of Magnesium Alloys
Metalworking: Bulk Forming
Electrochemical Techniques for In-Service Corrosion Monitoring
Corrosion: Fundamentals, Testing, and Protection
Surface Preparation
Protective Organic Coatings
CAD/CAM Applications in Machining
Machining