Electropolishing is an electrochemical process that involves anodic dissolution of a metal specimen (anode electrode) in an electrolytic cell. This article reviews the two-electrode and three-electrode systems for electropolishing. It presents the equations of anodic reactions and the selection criteria of electrolyte for electropolishing. The article also describes the mechanism of electropolishing and the effect of electropolishing on properties of metals.
Sign in
ASM members
Member Sign InM. Ziomek-Moroz, Electropolishing, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 139–142, https://doi.org/10.31399/asm.hb.v13a.a0003595
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.