Corrosion: Fundamentals, Testing, and Protection
Atmospheric Corrosion
-
Published:2003
Abstract
This article discusses the elements necessary for a galvanic cell operation. Detailed information on the possible corrosion reaction as a function of aqueous electrolyte concentration and pH, in the presence of certain ions, are provided using Pourbaix diagrams. A variety of atmospheric factors, climatic conditions, and air-chemical pollutants that determine the corrosiveness of the atmosphere and contribute to the metal corrosion process are discussed. The article reviews the phenomenon of precipitation runoff on the corroded metal surface and the corrosive microbial effect on metals. It describes the thermodynamics of atmospheric corrosion and models for predicting the corrosion damage of...
Sign in
ASM members
Member Sign InLucien Veleva, Russell D. Kane, Atmospheric Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 196–209, https://doi.org/10.31399/asm.hb.v13a.a0003606
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.