Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
-
Published:2003
Abstract
This article provides an overview of the metallurgical effects on corrosion of different series of aluminum alloys (1xxx, 2xxx, 3xxx, 4xxx, 5xxx, 6xxx, and 7xxx) that are classified into two categories. The first category includes the effects from insoluble, intermetallic constituent particles generally formed from trace impurity elements that play a predominant role in pitting corrosion. The second category comprises the effects from precipitation of secondary phases and effects from solute remaining in solid solution on corrosion of aluminum.
Sign in
ASM members
Member Sign InJim Moran, Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 275–278, https://doi.org/10.31399/asm.hb.v13a.a0003618
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.