Corrosion: Fundamentals, Testing, and Protection
Potential Measurements with Reference Electrodes
-
Published:2003
Abstract
Electrode potential is a key parameter in the thermodynamic and kinetic processes that drive aqueous corrosion. This article discusses the complexities associated with measuring electrode potential and explains where and how to use reference electrodes to improve measurement accuracy. It describes a three-electrode approach that compensates for measurement error stemming from nonequilibrium conditions. It also examines electrode materials and behaviors and offers insights on selection and operating conditions.
Sign in
ASM members
Member Sign InE. Protopopoff, P. Marcus, Potential Measurements with Reference Electrodes, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 13–16, https://doi.org/10.31399/asm.hb.v13a.a0003592
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!