Introduction to Forms of Corrosion Available to Purchase
-
Published:2003
Abstract
Corrosion is classified into two categories: corrosion that is not influenced by any other process and corrosion that is influenced by another process such as the presence of stresses or erosion. This article discusses uniform corrosion, localized corrosion, metallurgically influenced corrosion, and microbiologically influenced corrosion, which fit under the classification of corrosion that is not influenced by any outside process. It also explains mechanically assisted degradation and environmentally induced cracking, which fit under the classification of corrosion that is influenced by an outside process.
Bernard S. Covino, Jr., Stephen D. Cramer, Introduction to Forms of Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 189, https://doi.org/10.31399/asm.hb.v13a.a0003603
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.