Corrosion: Fundamentals, Testing, and Protection
Methods of Corrosion Protection
-
Published:2003
Abstract
This article discusses the factors affecting corrosion behavior. It describes galvanic corrosion and its protection methods. The article also provides information on coatings and inhibitors, which are used in corrosion protection.
Abstract
This article discusses factors that influence the effect of alloying, metallurgical treatments, and mechanical treatments on the corrosion resistance of metallic materials, with schematic illustrations.
Abstract
This article addresses the general effects of the composition, mechanical treatment, surface treatment, and processing on the corrosion resistance of aluminum and aluminum alloys. There are five major alloying elements: copper, manganese, silicon, magnesium, and zinc, which significantly influence the properties...
Sign in
ASM members
Member Sign InMethods of Corrosion Protection, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.