Metallography and Microstructures of Case-Hardening Steel
-
Published:2004
Page range:
627 - 643
Abstract
This article discusses the metallography and microstructures of carburized, carbonitrided, and nitrided steels, with illustrations. It provides information on the widely used metallographic techniques including sectioning, mounting, grinding and polishing, and etching.
You do not currently have access to this chapter.
Citation
Metallography and Microstructures of Case-Hardening Steel, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 627–643, https://doi.org/10.31399/asm.hb.v09.a0003762
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Metallography and Microstructures of Lead and Its Alloys
Metallography and Microstructures
Metallographic Specimen Preparation
Metallographer’s Guide Practices and Procedures for Irons and Steels
Metallography and Microstructures of Zirconium, Hafnium, and Their Alloys
Metallography and Microstructures
Metallography
Inspection of Metals Understanding the Basics
Metallography and Microstructures of Low-Carbon and Coated Steels
Metallography and Microstructures
Metallography and Microstructures of Carbon and Low-Alloy Steels
Metallography and Microstructures
Preparation and Microstructural Analysis of High-Performance Ceramics
Metallography and Microstructures
Metallography and Microstructures of Heat-Resistant Alloys
Metallography and Microstructures
Metallographic Technique for Nonferrous Metals and Special-Purpose Alloys
Metals Handbook Desk Edition (2nd Edition)
Metallography and Microstructures of Tin and Tin Alloys
Metallography and Microstructures