Analysis of the Effects of Lightning Strikes on Polymeric Composites[1]
-
Published:2004
Abstract
Lightning damage in polymer composites is manifested by damage at both the macroscopic or visual level and within the material microstructure. This article illustrates the effects of the laboratory-generated lightning strikes on polymeric composites.
You do not currently have access to this chapter.
Citation
Brian S. Hayes, Luther M. Gammon, Analysis of the Effects of Lightning Strikes on Polymeric Composites, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, https://doi.org/10.31399/asm.hb.v09.a0009085
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
The Effects of Lightning Strikes on Polymeric Composites
Optical Microscopy of Fiber-Reinforced Composites
Surface Degradation of Composites
Optical Microscopy of Fiber-Reinforced Composites
Wear Failures of Reinforced Polymers
Characterization and Failure Analysis of Plastics
The Failure Analysis Process
Fatigue and Fracture Understanding the Basics
Metallographic Techniques for Tool Steels
Metallography and Microstructures
Pipeline Failure Results from Lightning Strike: Act of Mother Nature?
Handbook of Case Histories in Failure Analysis
Examination of Damage and Material Evaluation
Failure Analysis and Prevention (2021 Edition)
Examination of Damage and Material Evaluation
Failure Analysis and Prevention
Fatigue Fracture Appearances
Failure Analysis and Prevention