Metallographic Techniques for Tool Steels
-
Published:2004
Abstract
Tool steels are prepared for metallographic examination in the same way as carbon steels with a few variations owing to hardness and alloying differences. This article explains what makes tool steels different and how to compensate for it when sectioning, mounting, grinding, polishing, and etching. It provides information and data on composition, hot working, austenitizing, tempering, and powder metal manufacturing and explains how it affects tool steel microstructure, using more than 100 detailed images.
Sign in
ASM members
Member Sign InGeorge F. Vander Voort, Metallographic Techniques for Tool Steels, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 644–669, https://doi.org/10.31399/asm.hb.v09.a0003766
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.