Spinodal Transformation Structures Available to Purchase
By
-
Published:2004
Page range:
140 - 143
Abstract
Spinodal transformation is a phase-separation reaction that occurs from kinetic behavior. This article discusses the theory of spinodal decomposition, and outlines the methods used in the characterization of spinodal structures in metal matrices.
You do not currently have access to this chapter.
Citation
Shane Para, Spinodal Transformation Structures, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 140–143, https://doi.org/10.31399/asm.hb.v09.a0003732
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Introduction to Phase Transformations
Elements of Metallurgy and Engineering Alloys
Intermediate Phases
Alloy Phase Diagrams
Glossary of Terms: Metallography and Microstructure
Metallography and Microstructures
Abbreviations and Symbols: Metallography and Microstructure
Metallography and Microstructures
Microstructure
Metallography Principles and Practice
Failure and Refurbishment
Superalloys: A Technical Guide (Second Edition)
Ductile Fracture
Understanding How Components Fail (Third Edition)
Tempering of Steel
Steels: Processing, Structure, and Performance (Second Edition)
Brief Glossary of Terms
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Some Additional Microstructural Information
Superalloys: A Technical Guide (Second Edition)