Abstract
This article provides information on the general structural features and origins of metals. The characteristic structural features of single-phase metals and alloys, such as grain structure and substructure, are discussed. The article also describes the major types of multiphase structures and macrostructure of metals and alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Introduction to Structures in Metals, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 23–28, https://doi.org/10.31399/asm.hb.v09.a0003721
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Introduction to Transformation Structures
Metallography and Microstructures
Bainitic Structures
Metallography and Microstructures
Periodic Table of Elements
Fundamentals of Modeling for Metals Processing
Massive Transformation Structures
Metallography and Microstructures
Solidification Structures of Steels and Cast Irons
Metallography and Microstructures
Voltammetry
Materials Characterization
Mössbauer Spectroscopy
Materials Characterization
Ion Chromatography
Materials Characterization
Introduction: Atlas of Fractographs
Fractography
Small-Angle X-Ray and Neutron Scattering
Materials Characterization