ASM Handbook
Metallography and Microstructures
Edited by
ASM International
Volume
9
ISBN electronic:
978-1-62708-177-1
Publication date:
2004
Abstract
This article is a comprehensive collection of tables listing: dangerous reactions of chemicals and designations of etchants; chemical-polishing solutions for irons and steels and nonferrous materials; attack-polishing solutions, macrostructure etchants for iron and steel; and major microstructure etchants for common phases and constituents in ferrous materials.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Tables of Chemicals and Etchants, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 1094–1114, https://doi.org/10.31399/asm.hb.v09.a0003764
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Glossary of Terms: Surface Engineering
Surface Engineering
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Introduction to Steels and Cast Irons
Metallographer’s Guide Practices and Procedures for Irons and Steels
Glossary
Metallographer’s Guide Practices and Procedures for Irons and Steels
Tables Helpful to the Metallographer
Metallographer’s Guide Practices and Procedures for Irons and Steels
Fundamentals of the Heat Treating of Steel
Practical Heat Treating (Second Edition)
Microstructures of Nitrided Iron and Steel
Practical Nitriding and Ferritic Nitrocarburizing
Free Energy of Pure Substances
Thermodynamics of Microstructures
Microbiologically Influenced Corrosion
Corrosion: Fundamentals, Testing, and Protection
Fundamentals of Steel Heat Treatment
Practical Heat Treating Basic Principles