Metallography and Microstructures
Metallography and Microstructures of Ceramics, Composite-Metal Forms, and Special Purpose Alloys
-
Published:2004
Abstract
Metallography plays a significant role in the quality control of metals and alloys used in the manufacture of implantable surgical devices. This article provides information and data on metallographic techniques along with images showing the microstructure of biomedical orthopedic alloys, including stainless steels, cobalt-base alloys, titanium and titanium alloys, porous coatings, and emerging materials.
Abstract
Microstructural analysis of specialized types of magnetic materials is centered on the examination of optical, electron, and scanning probe metallographic techniques unique to magnetic materials. This article provides a comprehensive overview of magnetic materials, their characteristics and sample preparation procedures. It reviews the methods...
Sign in
ASM members
Member Sign InMetallography and Microstructures of Ceramics, Composite-Metal Forms, and Special Purpose Alloys, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.