Metallography and MicrostructuresAvailable to Purchase
Volume 9 is a comprehensive guide to metallography and its application in product design and manufacturing. It provides detailed information on a wide range of metallographic techniques and how to interpret the microstructure and phase constituents commonly found in metals and alloys used throughout industry. It addresses composition, sample preparation, imaging technology, and analysis. It also explains what metallography and micrographs reveal about metallurgical processes, such as solidification and solid-state transformations, that drive microstructure development and influence material properties. The volume covers cast irons, carbon and low-alloy steels, tool steels, and stainless steels as well as aluminum, titanium, and precious-metal alloys. It also covers ceramics and cemented carbides, and examines special cases such as thermal spray coatings and powder metallurgy alloys. For information on the print version of Volume 9, ISBN 978-0-87170-706-2, follow this link.
Download citation file:
Table of Contents
-
Introduction
-
Laboratory Safety in MetallographyPublished:01 December 2004
-
Metallurgy and Microstructure
-
Physical Metallurgy Concepts in Interpretation of MicrostructuresByPublished:01 December 2004
-
Fundamentals of SolidificationByDoru M. Stefanescu;Doru M. StefanescuThe University of AlabamaSearch for other works by this author on:Roxana RuxandaRoxana RuxandaThe University of AlabamaSearch for other works by this author on:Published:01 December 2004
-
Solidification Structures of Steels and Cast IronsByDoru M. Stefanescu;Doru M. StefanescuThe University of AlabamaSearch for other works by this author on:Roxana RuxandaRoxana RuxandaThe University of AlabamaSearch for other works by this author on:Published:01 December 2004
-
Solidification Structures of Aluminum AlloysByDoru M. Stefanescu;Doru M. StefanescuThe University of AlabamaSearch for other works by this author on:Roxana RuxandaRoxana RuxandaThe University of AlabamaSearch for other works by this author on:Published:01 December 2004
-
Solidification Structures of Titanium AlloysByDoru M. Stefanescu;Doru M. StefanescuUniversity of AlabamaSearch for other works by this author on:Roxana RuxandaRoxana RuxandaUniversity of AlabamaSearch for other works by this author on:Published:01 December 2004
-
Computer Modeling of Solidification MicrostructuresByDoru M. Stefanescu;Doru M. StefanescuThe University of AlabamaSearch for other works by this author on:Roxana RuxandaRoxana RuxandaThe University of AlabamaSearch for other works by this author on:Published:01 December 2004
-
Introduction to Transformation StructuresByArnold R. MarderArnold R. MarderDepartment of Materials Science and Engineering, Lehigh UniversitySearch for other works by this author on:Published:01 December 2004
-
Structures by Precipitation from Solid SolutionByPublished:01 December 2004
-
Spinodal Transformation StructuresByPublished:01 December 2004
-
Ordered StructuresByJonathan ReginaJonathan ReginaLehigh UniversitySearch for other works by this author on:Published:01 December 2004
-
Massive Transformation StructuresPublished:01 December 2004
-
Bainitic StructuresByMatthew J. PerriconeMatthew J. PerriconeLehigh UniversitySearch for other works by this author on:Published:01 December 2004
-
Interdiffusion StructuresByPublished:01 December 2004
-
Plastic Deformation StructuresByDarcy A. Hughes;Darcy A. HughesSandia National LaboratoriesSearch for other works by this author on:Niels HansenNiels HansenRisø National LaboratorySearch for other works by this author on:Published:01 December 2004
-
Recovery, Recrystallization, and Grain-Growth StructuresByWilliam L. MankinsWilliam L. MankinsMetallurgical Services Incorporated
Revising author
Search for other works by this author on:Published:01 December 2004 -
Textured StructuresByDavid P. FieldDavid P. FieldWashington State UniversitySearch for other works by this author on:Published:01 December 2004
-
Metallographic Techniques
-
Metallographic Sectioning and Specimen ExtractionByDebbie AliyaDebbie AliyaAliya Analytical, Inc.Search for other works by this author on:Published:01 December 2004
-
MacroetchingBySamuel M. PurdySamuel M. PurdyNational Steel Corp.
Retired
Search for other works by this author on:Published:01 December 2004 -
Light and Electron Microscopy[1]ByPeter J. Goodhew;Peter J. GoodhewUniversity of LiverpoolSearch for other works by this author on:John Humphreys;John HumphreysManchester Materials CentreSearch for other works by this author on:Richard BeanlandRichard BeanlandMarconi Materials TechnologySearch for other works by this author on:Published:01 December 2004
-
Light MicroscopyByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.Search for other works by this author on:Published:01 December 2004
-
Scanning Electron MicroscopyByS. WeinbruchS. WeinbruchDarmstadt University of TechnologySearch for other works by this author on:Published:01 December 2004
-
Digital ImagingBySidnei Paciornik;Sidnei PaciornikCatholic University of Rio de JaneiroSearch for other works by this author on:Marcos Henrique de Pinho MauricioMarcos Henrique de Pinho MauricioCatholic University of Rio de JaneiroSearch for other works by this author on:Published:01 December 2004
-
Quantitative Image AnalysisByLeszek Wojnar;Leszek WojnarKraków University of Technology,Kraków,PolandSearch for other works by this author on:Krzysztof J. Kurzydłowski;Krzysztof J. KurzydłowskiWarsaw University of Technology,Warsaw,PolandSearch for other works by this author on:Janusz SzalaJanusz SzalaSilesian University of Technology,Katowice,PolandSearch for other works by this author on:Published:01 December 2004
-
Quantitative Characterization and Representation of Global Microstructural GeometryByArun M. GokhaleArun M. GokhaleGeorgia Institute of TechnologySearch for other works by this author on:Published:01 December 2004
-
Three-Dimensional MicroscopyByM.V. Kral;M.V. KralUniversity of Canterbury,Christchurch,New ZealandSearch for other works by this author on:M.D. Uchic;M.D. UchicWright-Patterson Air Force Research LaboratorySearch for other works by this author on:R.O. RosenbergR.O. RosenbergNaval Research LaboratorySearch for other works by this author on:Published:01 December 2004
-
Metallography of Archaeological AlloysByM.L. WaymanM.L. WaymanUniversity of AlbertaSearch for other works by this author on:Published:01 December 2004
-
Field Metallography TechniquesByBruce L. Bramfitt;Bruce L. BramfittInternational Steel Group, Inc.Search for other works by this author on:Samuel J. LawrenceSamuel J. LawrenceInternational Steel Group, Inc.Search for other works by this author on:Published:01 December 2004
-
Color MetallographyByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.Search for other works by this author on:Published:01 December 2004
-
-
Metallography and Microstructures of Ferrous Alloys
-
Metallography and Microstructures of Cast IronByJanina M. RadzikowskaJanina M. RadzikowskaThe Foundry Research Institute,Kraków,PolandSearch for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Low-Carbon and Coated SteelsByBruce L. BramfittBruce L. BramfittInternational Steel Group, Inc.Search for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Carbon and Low-Alloy Steels[1]ByBruce L. Bramfitt;Bruce L. BramfittInternational Steel Group, Inc.Search for other works by this author on:Samuel J. LawrenceSamuel J. LawrenceInternational Steel Group, Inc.Search for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Case-Hardening SteelPublished:01 December 2004
-
Metallographic Techniques for Tool SteelsByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.Search for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Stainless Steels and Maraging Steels[1]ByGeorge F. Vander Voort;George F. Vander VoortBuehler Ltd.Search for other works by this author on:Elena P. ManilovaElena P. ManilovaPolzunov Central Boiler and Turbine Institute,St. Petersburg,RussiaSearch for other works by this author on:Published:01 December 2004
-
Austenitic Manganese Steel CastingsBySelçuk KuyucakSelçuk KuyucakCANMET, Department of Natural Resources Canada
Revising author
Search for other works by this author on:Published:01 December 2004
-
-
Metallography and Microstructures of Nonferrous Alloys
-
Metallographic Techniques for Aluminum and Its AlloysByMałgorzata WarmuzekMałgorzata WarmuzekFoundry Research Institute,Kraków,PolandSearch for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Beryllium, Copper-Beryllium, and Nickel-Beryllium AlloysByPublished:01 December 2004
-
Metallography and Microstructures of Cobalt and Cobalt AlloysByD. Klarstrom;D. KlarstromHaynes International, Inc.
Revising author
Search for other works by this author on:P. Crook;P. CrookHaynes International, IncRevising author
Search for other works by this author on:J. WuJ. WuDeloro Stellite Group LimitedRevising author
Search for other works by this author on:Published:01 December 2004 -
Metallography and Microstructures of Copper and Its AlloysByR.N. Caron;R.N. CaronOlin Brass, Division of Olin Corporation
Revising author
Search for other works by this author on:R.G. Barth;R.G. BarthOlin Brass, Division of Olin CorporationRevising author
Search for other works by this author on:D.E. TylerD.E. TylerOlin Brass, Division of Olin CorporationRevising author
Search for other works by this author on:Published:01 December 2004 -
Metallography and Microstructures of Lead and Its AlloysPublished:01 December 2004
-
Metallography and Microstructures of Magnesium and Its AlloysByToby V. PadfieldToby V. PadfieldZF Sachs Automotive of AmericaSearch for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Nickel and Nickel-Copper AlloysByWilliam L. MankinsWilliam L. MankinsMetallurgical Services, Inc.Search for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Heat-Resistant AlloysByGeorge F. Vander Voort;George F. Vander VoortBuehler Ltd.Search for other works by this author on:Elena P. ManilovaElena P. ManilovaPolzunov Central Boiler and Turbine Institute,St. Petersburg,RussiaSearch for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Precious Metals and Precious Metal AlloysByElma van der Lingen;Elma van der LingenPhysical Metallurgy Division,Mintek,South AfricaSearch for other works by this author on:Lesley Cornish;Lesley CornishPhysical Metallurgy Division,Mintek,South AfricaSearch for other works by this author on:Stefanie Taylor;Stefanie TaylorPhysical Metallurgy Division,Mintek,South AfricaSearch for other works by this author on:Rainer Süss;Rainer SüssPhysical Metallurgy Division,Mintek,South AfricaSearch for other works by this author on:Stewart GriceStewart GriceHoover & Strong Inc.Search for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Refractory Metals and AlloysPublished:01 December 2004
-
Metallography and Microstructures of Tin and Tin AlloysPublished:01 December 2004
-
Metallography and Microstructures of Titanium and Its AlloysByCharles W. DombyCharles W. DombyThe Boeing CompanySearch for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Uranium and Its AlloysByHenry E. Fairman;Henry E. FairmanDepartment of Energy Feed Materials Production Center
Revising author
Retired
Search for other works by this author on:Ann KellyAnn KellyLos Alamos National LaboratorySearch for other works by this author on:Published:01 December 2004 -
Metallography and Microstructures of Zinc and Its AlloysPublished:01 December 2004
-
Metallography and Microstructures of Zirconium, Hafnium, and Their AlloysByPaul E. Danielson;Paul E. DanielsonAlbany Research Center, U.S. Department of EnergySearch for other works by this author on:Richard C. SutherlinRichard C. SutherlinWah Chang, An Allegheny Technologies CompanySearch for other works by this author on:Published:01 December 2004
-
-
Metallography and Microstructures of Ceramics, Composite-Metal Forms, and Special Purpose Alloys
-
Metallography of Biomedical Orthopedic AlloysPublished:01 December 2004
-
Microstructure and Domain Imaging of Magnetic MaterialsByMatthew A. Willard;Matthew A. WillardNaval Research LaboratorySearch for other works by this author on:George F. Vander VoortGeorge F. Vander VoortBuehler Ltd.Search for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Powder Metallurgy AlloysByLeander F. Pease, III;Leander F. Pease, IIIPowder-Tech Associates, Inc.Search for other works by this author on:Douglas L. PeaseDouglas L. PeasePowder-Tech Associates, Inc.Search for other works by this author on:Published:01 December 2004
-
Metallography and Microstructures of Semisolid Formed AlloysPublished:01 December 2004
-
Microstructural Characterization of Thermal Spray CoatingsByPublished:01 December 2004
-
Preparation and Microstructural Analysis of High-Performance CeramicsByUlrike Täffner;Ulrike TäffnerMax-Planck-Institut für Metallforschung,Stuttgart,GermanySearch for other works by this author on:Veronika Carle;Veronika CarleMax-Planck-Institut für Metallforschung,Stuttgart,GermanySearch for other works by this author on:Ute Schäfer;Ute SchäferMax-Planck-Institut für Metallforschung,Stuttgart,GermanySearch for other works by this author on:Michael J. HoffmannMichael J. HoffmannInstitut für Keramik im Maschinenbau, Universität Karlsruhe,GermanySearch for other works by this author on:Published:01 December 2004
-
Metallography of Cemented CarbidesPublished:01 December 2004
-
-
Optical Microscopy of Fiber-Reinforced Composites
-
Publication Information for Optical Microscopy of Fiber-Reinforced Composites[1]Published:01 December 2004
-
Introduction—Composite Materials and Optical Microscopy[1]Published:01 December 2004
-
Sample Preparation and Mounting for Fiber-Reinforced Composites[1]Published:01 December 2004
-
Rough Grinding and Polishing of Fiber-Reinforced Composite Samples[1]Published:01 December 2004
-
Special Sample Preparation and Polishing for Fiber-Reinforced Composites[1]Published:01 December 2004
-
Viewing Composite Specimens Using Reflected Light Microscopy[1]Published:01 December 2004
-
Composite Structure Analysis[1]Published:01 December 2004
-
Void Analysis of Composite Materials[1]Published:01 December 2004
-
Microcrack Analysis of Composite Materials[1]Published:01 December 2004
-
Toughening Methods for Thermoset-Matrix Composites[1]Published:01 December 2004
-
Impact Response of Composites[1]Published:01 December 2004
-
Matrix Microstructure Analysis of Fiber-Reinforced Composites[1]Published:01 December 2004
-
Analysis of Honeycomb-Cored Sandwich Structure Composites[1]Published:01 December 2004
-
Analysis of Surface Degradation of Composites[1]Published:01 December 2004
-
Analysis of the Effects of Lightning Strikes on Polymeric Composites[1]Published:01 December 2004
-
-
Supplementary Information
-
Glossary of Terms: Metallography and MicrostructurePublished:01 December 2004
-
Abbreviations and Symbols: Metallography and MicrostructurePublished:01 December 2004