This article is a compilation of more than 35 binary alloy phase diagrams for which cobalt (Co) is the first named element in the binary pair. The diagrams plot alloy composition in terms of weight percent, while indicating atomic percent along a secondary scale. Each diagram is accompanied by a table of crystallographic data that includes composition ranges as well as the Pearson symbol, space group, and prototype for each phase.