Au (Gold) Ternary Alloy Phase Diagrams
-
Published:2016
Page range:
682
Abstract
This article is a compilation of ternary alloy phase diagrams for which gold (Au) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes five phase diagrams: Au-Cu-Ni boundaries of solid-state miscibility gap; Au-Cu-Ni liquidus projection; Au-Cu-Ni miscibility gap at 400 degrees centigrade; Au-Cu-Ni miscibility gap at 700 degrees centigrade; and Au-Sn-Te liquidus projection.
You do not currently have access to this chapter.
Citation
Au (Gold) Ternary Alloy Phase Diagrams, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 682, https://doi.org/10.31399/asm.hb.v03.a0006234
Download citation file:
Related Book Content
Cu (Copper) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Al (Aluminum) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Ge (Germanium) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
B (Boron) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Ag (Silver) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Pb (Lead) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Cd (Cadmium) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Fe (Iron) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Co (Cobalt) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Cr (Chromium) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams