Co (Cobalt) Ternary Alloy Phase Diagrams
-
Published:2016
Abstract
This article is a compilation of ternary alloy phase diagrams for which cobalt (Co) is the first-named element in the ternary system. The other elements are Cr, Cu, Fe, Mo, Ni, Ti, V, and W. The diagrams are presented with element compositions in weight percent. The article includes 36 phase diagrams (liquidus projection, solidus projection and isothermal section).
Co (Cobalt) Ternary Alloy Phase Diagrams, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 703–712, https://doi.org/10.31399/asm.hb.v03.a0006238