Pu (Plutonium) Binary Alloy Phase Diagrams
-
Published:2016
Abstract
This article is a compilation of binary alloy phase diagrams for which plutonium (Pu) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
Pu (Plutonium) Binary Alloy Phase Diagrams, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 569–571, https://doi.org/10.31399/asm.hb.v03.a0006196