Pb (Lead) Ternary Alloy Phase Diagrams
-
Published:2016
Abstract
This article is a compilation of ternary alloy phase diagrams for which lead (Pb) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 7 phase diagrams: Pb-Sb-Sn liquidus projection; Pb-Sb-Sn isothermal section at 240 °C; Pb-Sb-Sn isothermal section at 189 °C; Pb-Sb-Sn (Pb) liquidus projection; Pb-Sn-Zn liquidus projection; and Pb-Sn-Zn isothermal section at 532 °C.
Pb (Lead) Ternary Alloy Phase Diagrams, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 743–746, https://doi.org/10.31399/asm.hb.v03.a0006245