Sm (Samarium) Binary Alloy Phase Diagrams
-
Published:2016
Abstract
This article is a compilation of binary alloy phase diagrams for which samarium (Sm) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.
You do not currently have access to this chapter.
Citation
Sm (Samarium) Binary Alloy Phase Diagrams, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 600–601, https://doi.org/10.31399/asm.hb.v03.a0006206
Download citation file:
Related Book Content
Yb (Ytterbium) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
Zn (Zinc) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
Ta (Tantalum) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
Rh (Rhodium) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
Tb (Terbium) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
La (Lanthanum) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
Ru (Ruthenium) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
Te (Tellurium) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
S (Sulfur) Binary Alloy Phase Diagrams
Alloy Phase Diagrams
Th (Thorium) Binary Alloy Phase Diagrams
Alloy Phase Diagrams