Principles of Shearing, Blanking, and Piercing
-
Published:2006
Abstract
Many shearing, blanking, and piercing operations are based on the same underlying principles of shear mechanisms. This article provides information on the various operations associated with die cutting and describes three phases involved in the shear cutting or punching action. These phases include deformation, penetration and fracture. The article also explains the effect of clearance on tool life and force and power requirements. It reviews the forces involved in the punching process and describes the diameter of a hole or blank in relation to material thickness. The limitations of punching are also discussed. The article describes the relationship of...
Sign in
ASM members
Member Sign InPrinciples of Shearing, Blanking, and Piercing, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 28–38, https://doi.org/10.31399/asm.hb.v14b.a0005116
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.