This article provides an overview of the interfacial interactions with a lubricant film between a die and a metal, lubricant mechanisms, chemistry, qualification testing, application methods, and property test methods. It focuses on sheet metal-forming operations, although the discussions are relevant to metal-forming operations in general. The article also deals with lubricant selection as influenced by the metal to be formed and particular sheet-metal forming operations. The article also discusses some aspects of microbiology and toxicity in lubricants.
Selection and Use of Lubricants in Forming of Sheet Metal, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 248–264, https://doi.org/10.31399/asm.hb.v14b.a0005159
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.