Metalworking: Sheet Forming
Selection and Use of Lubricants in Forming of Sheet Metal
-
Published:2006
Abstract
This article provides an overview of the interfacial interactions with a lubricant film between a die and a metal, lubricant mechanisms, chemistry, qualification testing, application methods, and property test methods. It focuses on sheet metal-forming operations, although the discussions are relevant to metal-forming operations in general. The article also deals with lubricant selection as influenced by the metal to be formed and particular sheet-metal forming operations. The article also discusses some aspects of microbiology and toxicity in lubricants.
Sign in
ASM members
Member Sign InSelection and Use of Lubricants in Forming of Sheet Metal, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 248–264, https://doi.org/10.31399/asm.hb.v14b.a0005159
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.