Abstract
This article provides a detailed account of the process development, cutting principle, and components of the abrasive waterjet cutting process. The advantages of abrasive waterjet machining are summarized. The article also discusses the factors affecting the cut quality, and the applications and limitations of abrasive waterjet cutting.
Topics
Abrasive waterjet cutting
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Abrasive Waterjet Cutting, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 120–129, https://doi.org/10.31399/asm.hb.v14b.a0005107
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Machining
Titanium: A Technical Guide (Second Edition)
Cutting Operations
Metalworking: Sheet Forming
2011 and 2012 Free Machining Aluminum Alloy
Properties and Selection of Aluminum Alloys
Waterjet/Abrasive Waterjet Machining
Machining
Microstructure and Machinability
Metals Handbook Desk Edition (2nd Edition)
Machining of Carbon and Alloy Steels
Machining
Elements of the Machining Process
Metals Handbook Desk Edition (2nd Edition)
Laser Cutting, Drilling, and Shock Peening
Welding Fundamentals and Processes