Abstract
This article discusses the principles of the press-brake forming process and its applicability with an example. It describes the types of press brakes and examines some considerations, which help in the selection of machine. The article provides information on flattening dies, gooseneck punches, wiping dies, channel dies, arbor-type punches, box-forming dies, curling dies, beading dies, and cam-driven dies, with illustrations. It discusses the tool material selection for various operations. The article explains the procedures used for producing different shapes, including simple boxlike parts, panels, flanged parts, architectural columns, fully closed parts, and semicircular parts. It examines the effect of...
Sign in
ASM members
Member Sign InPress-Brake Forming, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 307–318, https://doi.org/10.31399/asm.hb.v14b.a0005177
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.