Press Brakes Available to Purchase
-
Published:2006
Abstract
Press brakes are a common and versatile type of equipment for bending metal by delivering an accurate vertical force in a confined longitudinal area. This article begins with a discussion on the design, widening methods, and types of materials used in press brakes. It focuses on the two basic drive systems used in operating press brakes, namely, mechanical and hydraulic drive systems. The article also provides an outline on the tooling associated with press-brakes.
Press Brakes, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 212–220, https://doi.org/10.31399/asm.hb.v14b.a0005113