Metal spinning is a term used to describe the forming of metal into seamless, axisymmetric shapes by a combination of rotational motion and force. This article describes two forming techniques, such as manual spinning and power spinning, for forming seamless metal components. The process technology, equipment, and tooling for both manual spinning and power spinning are also discussed.