Nonferrous Hardness Conversions
-
Published:2006
Abstract
This article is a comprehensive collection of tables that list the approximate equivalent hardness numbers for wrought aluminum products, wrought coppers, and cartridge brass.
You do not currently have access to this chapter.
Citation
Nonferrous Hardness Conversions, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 898–900, https://doi.org/10.31399/asm.hb.v14b.a0005185
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Nonferrous Hardness Conversions
Metalworking: Bulk Forming
Alloy and Temper Designation Systems for Aluminum and Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Steel Hardness Conversions
Metalworking: Bulk Forming
Surface Engineering to Change the Surface Metallurgy
Surface Engineering for Corrosion and Wear Resistance
Steel Hardness Conversions
Heat Treating of Irons and Steels
Properties of Wrought Aluminum Alloys
Metals Handbook Desk Edition (2nd Edition)
Properties of Wrought Aluminum and Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials