Stretch forming is the forming of sheet, bars, and rolled or extruded sections over a die or form block of the required shape while the workpiece is held in tension. This article discusses the applicability, advantages, and machines and accessories of stretch forming. It provides a detailed discussion on four methods of stretch forming, namely, stretch draw forming, stretch wrapping, compression forming, and radial draw forming.