Abstract
This article begins with a discussion on the energy sources used for thermal forming. These include electric induction coil, gas flame, plasma torch, and laser beam. The article discusses the mechanisms of forming and different modes of deformation. It describes the effect of process and material parameters on forming and the effect of metallurgical changes on mechanical property and microstructure of stainless steel. The article concludes with information on the applications of thermal forming.
You do not currently have access to this chapter.
Citation
Alan Male, Thermal Forming of Sheet and Plate, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 424–428, https://doi.org/10.31399/asm.hb.v14b.a0005130
Download citation file:
Related Book Content
Alclad 2029 High-Strength, High-Toughness Sheet/Plate
Properties and Selection of Aluminum Alloys
Shearing of Sheet, Strip, and Plate
Metalworking: Sheet Forming
Forming
Stainless Steels for Design Engineers
Energy Sources Used for Fusion Welding
Welding, Brazing, and Soldering
Weld Procedure Qualification
Welding, Brazing, and Soldering
Roll Welding and Laser Roll Welding
Welding Fundamentals and Processes
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)
Brief Glossary of Terms
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Pultrusion
Engineered Materials Handbook Desk Edition
High-Temperature Applications
Composites