Metalworking: Sheet Forming
Deep Drawing
Revising author
-
Published:2006
Abstract
This article illustrates the mechanics of the deep drawing of a cylindrical cup. It discusses the fundamentals of drawing and drawability. Sheet metal is drawn in either hydraulic or mechanical presses. The article summarizes the defects in drawing and factors considered in press selection for drawing. It explains the types of dies used for drawing sheet metal and the effects of process variables and material variables on deep drawing. The process variables that affect the success or failure of a deep-drawing operation include the punch and die radii, punch-to-die clearance, press speed, lubrication, and type of restraint of metal...
Sign in
ASM members
Member Sign InMahmoud Y. Demeri, Deep Drawing, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 319–336, https://doi.org/10.31399/asm.hb.v14b.a0005121
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.