Straightening of Bars, Shapes, and Long Parts
-
Published:2006
Abstract
Bars, structural shapes, and long parts are straightened by bending, twisting, or stretching. This article describes the straightening of bars, shapes, and long parts by material displacement, heating, and presses. It explains the process of parallel-roll straightening, automatic press roll straightening, moving-insert straightening, parallel-rail straightening, and epicyclic straightening. The article concludes with a discussion on straightening in bar production.
Topics
Bars,
Rods and wires,
Tubes,
Blanking,
Shearing,
Bending,
Sheet forming,
Press forming,
Spinning,
Machine tools and manufacturing equipment,
Presses,
Straightening,
Epicyclic straightening,
Material displacement straightening,
Moving-insert straightening,
Parallel-rail straightening,
Roll straightening,
Stretch forming
You do not currently have access to this chapter.
Citation
Straightening of Bars, Shapes, and Long Parts, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 472–482, https://doi.org/10.31399/asm.hb.v14b.a0005136
Download citation file:
Related Book Content
Forming of Bars, Tube, and Wire
Metals Handbook Desk Edition (2nd Edition)
Forming of Advanced High-Strength Steels (AHSS)
Sheet Metal Forming Processes and Applications
Forming of Steel Tailor-Welded Blanks
Metalworking: Sheet Forming
Wear and Lubrication of Sheet-Metal Forming Dies
Metalworking: Sheet Forming
Straightening of Tubing
Metalworking: Sheet Forming
Design for Sheet Forming
Metalworking: Sheet Forming
Practical Aspects of Converting Ingot to Billet
Metalworking: Bulk Forming
Failure of a Press
ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions
Shearing of Bars and Bar Sections
Metalworking: Sheet Forming
Damaged Propeller Blades
ASM Failure Analysis Case Histories: Air and Spacecraft