Design for Sheet Forming
-
Published:2006
Abstract
Sheet-forming processes provide considerable geometric and material flexibility in meeting these requirements, and design of parts for sheet forming must take into account these benefits as well as the limitations of the processes. This article reviews the basic forming operations and their general geometric features. These operations include hole making, flanging, bead and rib forming, and stretching and drawing for shallow or deep recesses. The article illustrates the general approach to design for sheet forming and the considerations that must be made for material savings and manufacturing ease, in addition to part function. It concludes with information on reducing...
Sign in
ASM members
Member Sign InHoward Kuhn, Design for Sheet Forming, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 11–19, https://doi.org/10.31399/asm.hb.v14b.a0005101
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.