Fatigue Crack Growth Testing Available to Purchase
-
Published:1996
Abstract
This article describes the fracture mechanics in fatigue. It discusses the fatigue crack growth rate (FCGR) testing that consists of several steps, beginning with selecting the specimen size, geometry, and crack length measurement technique. The two major aspects of FCGR test analysis are to ensure suitability of the test data and to calculate growth rates from the data. The article presents an analysis of the crack growth data. Optical, compliance, and electric potential difference are the most common laboratory techniques, and the article reviews their merits and limitations. Forced-displacement, forced-vibration, rotational-bending, resonance, and servomechanical systems for various loading conditions are also discussed.
Ashok Saxena, Christopher L. Muhlstein, Fatigue Crack Growth Testing, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 168–184, https://doi.org/10.31399/asm.hb.v19.a0002360
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.