Selecting Aluminum Alloys to Resist Failure by Fracture Mechanisms
-
Published:1996
Abstract
This article provides an overview of fatigue and fracture resistance of aluminum alloys. It discusses the characteristics of aluminum alloy classes and the fracture mechanics of aluminum alloys. The article tabulates relative stress-corrosion cracking ratings for high-strength wrought aluminum products. It analyzes the selection of various alloys for stress-corrosion cracking resistance, including aluminum-lithium alloys, copper-free 7XXX alloys, and casting alloys. The article presents a list of typical tensile properties and fatigue limit of aluminum alloys. It also describes the effects of composition, microstructure, thermal treatments, and processing in fatigue crack growth of aluminum alloys.
R.J. Bucci, G. Nordmark, E.A. Starke, Jr., Selecting Aluminum Alloys to Resist Failure by Fracture Mechanisms, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 771–812, https://doi.org/10.31399/asm.hb.v19.a0002406
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.