Elevated-Temperature Crack Growth Available to Purchase
-
Published:1996
Abstract
This article describes the concepts for characterizing and predicting elevated-temperature crack growth in structural materials. It discusses both creep and creep-fatigue crack growth and focuses mainly on creep crack growth tests that are carried out in accordance with ASTM E 1457. The article provides information on typical test procedures and equipment used for these tests. It concludes with information on crack growth correlations.
Richard H. Norris, Parmeet S. Grover, B. Carter Hamilton, Ashok Saxena, Elevated-Temperature Crack Growth, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 507–519, https://doi.org/10.31399/asm.hb.v19.a0002389