Fatigue and Fracture Behavior of Glasses
-
Published:1996
Abstract
This article discusses the fracture behavior of silicate glasses, more specifically, soda-lime-silicate glass, borosilicate glass and vitreous silica. It analyzes the testing and calculation of dynamic fatigue and slow-crack-growth for lifetime prediction of glasses. The article illustrates the phenomenon of static fatigue and concludes with a discussion on the role of surface damage in strength and fatigue behavior.