Fatigue and Fracture
Fracture and Fatigue of DRA Composites
-
Published:1996
Abstract
This article reviews the tensile properties and toughness characteristics of discontinuously reinforced aluminum (DRA) composites in terms of particle spacing, particle size, volume fraction, matrix alloy, and matrix microstructure. Both fracture toughness data and impact toughness data of the DRA composites are summarized. The article discusses the effects of confining pressure on the ductility of the DRA materials. It describes the fatigue behavior, such as stress-life behavior, strain-life behavior, and fatigue crack propagation, of the DRA.
Sign in
ASM members
Member Sign InJohn J. Lewandowski, Preet M. Singh, Fracture and Fatigue of DRA Composites, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 895–904, https://doi.org/10.31399/asm.hb.v19.a0002414
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!