Damage Tolerance Certification of Commercial Aircraft
-
Published:1996
Abstract
Damage tolerance is a philosophy used for maintaining the structural safety of commercial transport aircrafts. This article describes the structural evaluations necessary to comply with the regulations contained in the Federal Air worthiness Requirements 25.571 whose guidance is given in Advisory Circular 25.571-1A from the Federal Aviation Administration. It provides an overview of the historical evolution of damage tolerance philosophy and presents a discussion of the design philosophies and a summary of the evaluation tasks for damage tolerance certification.
Sign in
ASM members
Member Sign InT. Swift, Damage Tolerance Certification of Commercial Aircraft, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 566–576, https://doi.org/10.31399/asm.hb.v19.a0002393
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!