Fatigue and Fracture
Fatigue and Fracture Properties of Duplex Stainless Steels
-
Published:1996
Abstract
This article reviews the influence of local strains and corrosion fatigue on the initiation of fatigue cracks in duplex stainless steels. It provides useful information on fatigue crack growth, fatigue strength, and fracture toughness of duplex stainless steels. The article discusses the fatigue and fracture behavior of duplex stainless steels during stress-corrosion cracking. It details the elevated-temperature properties of duplex stainless steels, such as creep-fatigue behavior and thermal cycling properties.
R. Johansson, Fatigue and Fracture Properties of Duplex Stainless Steels, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 757–768, https://doi.org/10.31399/asm.hb.v19.a0002405
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.