Life Extension and Damage Tolerance of Aircraft
-
Published:1996
Abstract
This article describes two analysis methods that are used to determine the life of aircrafts: fatigue life and fracture mechanics methods. The life limiting factors that control the durability of the aircraft are also discussed. The article provides an overview of the various approaches to corrosion identification and prevention. These include safe-life, fail-safe, and damage tolerance approaches. The article discusses their application to the process of extending the life of aircraft structural components.
Sign in
ASM members
Member Sign InMitchell P. Kaplan, Timothy A. Wolff, Life Extension and Damage Tolerance of Aircraft, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 557–565, https://doi.org/10.31399/asm.hb.v19.a0002392
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!