This article provides information on the nominal compositions of high-carbon bearing steels and carburizing bearing steels. It discusses the bearing fundamentals with emphasis on surface contact, stresses, and fatigue life of bearings. The article describes bearing life prediction using three factors, namely, reliability, material, and application. It analyzes the bearing damage modes and concludes with information on fatigue failure considerations.