Statistical Considerations in Fatigue Available to Purchase
-
Published:1996
Abstract
There are two parts to deal with uncertainty in fatigue design: determining the distributions of possible values for all uncertain inputs and calculating the probability of failure due to all the uncertain inputs. This article discusses the sources of uncertainty in a fatigue analysis, such as the material properties, distribution of applied stress levels within a given environment, environments or loading intensities, and modeling or prediction. It presents a probabilistic approach for analyzing the uncertainties and determining the level of reliability (probability of failure).
Paul S. Veers, Statistical Considerations in Fatigue, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 295–302, https://doi.org/10.31399/asm.hb.v19.a0002369
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.