Countersinking, counterboring, and spotfacing operations can be carried out on drilling machines and usually follow drilling operations. This article discusses five common types of countersinking tools or countersinks, namely, machine, three-flute, single-flute, insert-type, and interchangeable countersinks. It provides a short description of the two types of spotfacing tools: back and double-end spotfacers and automatic back spotfacers. The article describes different types of counterboring tools, including interchangeable-pilot, integral-pilot, and interchangeable-cutter counterbores. It tabulates the nominal speeds and feeds for counterboring and spotfacing of carbon and low-alloy steels with high-speed steel and carbide tools.
Countersinking, Counterboring, and Spotfacing, Machining, Vol 16, ASM Handbook, By ASM Handbook Committee, ASM International, 1989, p 249–251, https://doi.org/10.31399/asm.hb.v16.a0002137
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.