Abstract
Cast cobalt alloys were developed to bridge the gap between high-speed steels and carbides. Although comparable in room-temperature hardness to high-speed steel tools, cast cobalt alloy tools retain their hardness to a much higher temperature and can be used at higher cutting speeds than high-speed steel tools. This article provides an overview of the processing, properties, and applications of these alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Cast Cobalt Alloys, Machining, Vol 16, ASM Handbook, By ASM Handbook Committee, ASM International, 1989, p 69–70, https://doi.org/10.31399/asm.hb.v16.a0002123
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Planing
Machining
Shaping and Slotting
Machining
Etchants for Revealing Microstructure
Metallography Principles and Practice
Carbon Steel Heat Treating Problems
ASM Failure Analysis Case Histories: Processing Errors and Defects
Tool Steels
Steel Metallurgy for the Non-Metallurgist
Severe General Corrosion on Historic Lane Plate Made From Chromium Steel
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Cast Steel Housing with Grain Boundary Precipitates
ASM Failure Analysis Case Histories: Processing Errors and Defects
Production of Ductile Iron Castings
Cast Iron Science and Technology
Failure of an Incoloy 800 Piping System
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms